Heat treatment

In order to achieve the desired degree of hardness of our gears, the components are conventionally hardened after carburizing at 900°C in an oil bath, whereby the structural transformation during quenching at 80°C produces the required surface hardness. The parts are then cleaned of oil in a chamber washing machine and tempered at around 180°C to achieve the optimum hardness.